氩弧焊丝

不锈钢氩弧及埋弧焊丝










Stainless Steel   Argonarc and Submerged Arc Electrode Wires






 










牌号规格熔敷金属标准或典型化学成分(%)
主要用途
Standard   &Typical Chemical Composition of Deposited Metal
Brand NameSpecification                     (mm)CSiMnPSCrNiMo其它Applications
ER304(H1Cr18Ni9)1.0-5.0≤0.14≤0.601.00-2.00≤0.030≤0.03018.00-20.008.00-10.00__此牌号应用很广,它具有良好的在硝酸、大部分有机酸和无机酸水溶液、磷酸、碱及煤气等介质中的耐腐蚀性。适用于制造建筑用的装饰部件、不锈耐酸外壳及容器、阀、管道等不锈钢材的焊接。
Widely utilized Excellent resisting capacity to nitric   acid,water solution of most organic and inorganic acids,phosphoric   acid,alkali and coal gas.Suitable for the welding of stainless steel for   decoration parts of construction,acid resisting shells,containers,values and   pipes.
ER308(H0Cr21Ni10)1.0-5.0≤0.08≤0.601.00-2.50≤0.030≤0.03019.50-22.509.00-11.00__适用于SUS304系不锈钢焊接,配用中性烧结焊剂,其中添加适量的合金元素,可使焊道中的金属成分稳定的维持在一定适当的含量。焊后的焊道具有优良的耐龟裂、耐腐蚀、焊渣剥离性好,焊道平滑,适用于制造食品设备、化工设备和原子工业设备上的部件焊接。
ER308L(H00Cr21Ni10)1.0-5.0≤0.03≤0.601.00-2.50≤0.030≤0.02019.50-22.509.00-11.00__308L为低含碳量焊丝,故焊道本身的耐龟裂、抗粒间腐蚀性及延展性较308焊丝好。
Low carbon rod Better chap and inter-crystal corrosion resisting   and elongation capacity than 308 rod.
ER309(H1Cr24Ni13)1.0-5.0≤0.12≤0.601.00-2.50≤0.030≤0.03023.00-25.0012.00-14.00__用于Cr22-Ni12(SUS309)系不锈钢焊接,配用中性烧结焊剂施焊,可得到稳定的焊道合金成分和优良的机械性能。焊渣剥离性好,焊道平滑。
For the welding of Cr22-Ni12(SUS309)series stainless   steel.Equipped with neutral agglomerated flux for welding.Stable welding   lines alloy component and excellent mechanical perfofmance.Easy to remove   welding residues with smooth welding lines.
ER310(H1Cr26Ni21)1.0-5.0≤0.15≤0.601.00-2.50≤0.030≤0.03025.00-28.0020.00-22.00__适合异种金属焊接和自硬性高的合金钢和高碳钢的连接。如:Cr25-Ni20
For the welding of special tyep metals and the connection   between high self-hardening alloy steel and high-carbon steel,such as   Cr25-Ni20.
ER316(H0Cr19Ni12Mo2)1.0-5.0≤0.08≤0.601.00-2.50≤0.030≤0.03018.00-20.0011.00-14.002.00-3.00_用于Cr18-Ni12(SUS316)系不锈钢焊接,配用中性烧结焊剂施焊,可得到稳定的焊道合金成分和优良的机械性能。焊渣剥离性好,焊道平滑。
For the welding of Cr18-Ni12(SUS316)series stainless   steel.Equipped with neutral agglomerated flux for welding.Stable welding   lines alloy component and excellent mechanical perfofmance.Easy to remove   welding residues with smooth welding lines.
ER316L(H00Cr19Ni12Mo2)1.0-5.0≤0.03≤0.601.00-2.50≤0.030≤0.02018.00-20.0011.00-14.002.00-3.00_316L为低含碳量焊丝。适用于焊接尿素、合成纤维等设备和同类型不锈钢结构及焊后不能进行热处理的铬不锈钢及复合钢和异种钢等。
ER317(H0Cr19Ni14Mo3)1.0-5.0≤0.08≤0.601.00-2.50≤0.030≤0.03018.50-20.5013.00-15.003.00-4.00_高Cr,高Mo,具有耐腐蚀性、耐热性,抗硫酸、抗亚硫酸及有机酸,适用于重要化学容器的焊接。
high Cr and Mo Excellent performance on hole corrosion and heat   resisting.Sulphuric acid,sulfurous acid and organic acid resisting Suitable   for chemical containers.
ER321(H0Cr20Ni10Ti)1.0-5.0≤0.08≤0.601.00-2.50≤0.030≤0.03018.50-20.509.00-10.50_Ti 9×C%-1.00添加Ti,增强焊道的晶间腐蚀抵抗性,适用于重要耐腐蚀容器的焊接。
Added with Ti to improve the capacith of inter-crystal corrosion   resisting of welding lines.Suitable for corrosion-resisting containers.
ER347(H0Cr20Ni10Nb)1.0-5.0≤0.08≤0.601.00-2.50≤0.030≤0.03019.00-21.509.00-11.00_Nb 10×C%-1.00添加Nb阻止碳化铬沉淀,具有极佳的高温强度,特别适用于耐热钢的焊接。
Added with Nb to prevent the deposition of carborundum.Excellent   strength under high temperature.Suitable for heat-resising containers.
ER410(H1Cr13)1.0-5.0≤0.12≤0.50≤0.60≤0.030≤0.03011.50-13.50≤0.60__适用于Cr13马氏体钢的焊接,在高温下有优异的耐氧化性和耐腐蚀性。
For the welding of Cr13 martensitic steel.Excellent performance   of oxidation resisting under high temperature.
ER430(H1Cr17)1.0-5.0≤0.10≤0.50≤0.60≤0.030≤0.03015.50-17.00≤0.60__适用于Cr17铁素体钢的焊接,特别适用于硝酸容器的焊接。
For the welding of Cr17 ferritic steel,Especially suitable for   nitric acid containers.